Item | Unit | VT | ST | A competitor’s | B competitor’s |
Light transmittance (390nm—900um) | % | 91 | 91 | 90.2 | 90.1 |
Haze | % | 0.25 | 0.25 | 0.3 | 0.6 |
■ The excellent UV resistance property can maintain and extend the laminated glass ‘useful life .
■ ST film enjoy excellent weather durability than other competitors due to low degradation in the UV radiation .
Item | Unit | VT | ST | A competitor’s | B competitor’s |
Blocked UV wavelength | nm | 390 | 390 | 360 | 380 |
UV block rate | % | >99 | >99 | 50 | 90 |
Test method : fluorescent tube (UVA340, 50℃±5℃ ,HR65%)
150mm*75mm , glass + ST+glass
1) Heat &Humidity resistance test
Test time:1000hours
Condition :85℃ 85%RH
150mm*200mm glass + ST+glass
■ Under tough condition 85℃ 85%RH ,ST EVA has outstanding weather durability and stability
■ ST laminated glass has no obvious changes and edge defects
1) UV Blocking test
Test method : fluorescent tube (UVA340, 50℃±5℃ ,HR65%)
150mm*75mm , glass + ST+glass
■ The excellent UV resistance property can maintain and extend the laminated glass ‘useful life .
■ ST film enjoy excellent weather durability than other competitors due to low degradation in the UV radiation .
KENGO VT EVA
135℃ 60mins Crosslinking rate can reach to 94%